景观膜结构在安装及使用过程中,经常会出现一些小问题,如安装时在地面或其它构筑物上拖动的磨损、尖锐物体划伤或刺破、膜材吊装或张拉时的意外撕裂,使用过程中高空坠物击破或人为破坏等等,而这些情况一旦发生,需及时处理的。下面山东膜结构厂家就来讲讲景观膜结构膜面破损的处理方式。
In the process of installation and use of landscape membrane structures, some small problems often occur, such as wear caused by dragging on the ground or other structures during installation, scratches or punctures caused by sharp objects, accidental tears caused by lifting or tensioning of membrane materials, damage caused by falling objects or man-made damage during use, etc. Once these situations occur, they need to be handled in a timely manner. Next, Shandong membrane structure manufacturers will talk about the treatment of damage to the membrane surface of landscape membrane structures.
一、膜结构破损以及处理工作:
1、 Membrane structure damage and treatment:
1、如果仅仅是局部膜材的表面涂层磨损、基布织物的纤维完好,可用高性能透明胶粘贴或热合在磨损区域。
1. If only the surface coating of local membrane material is worn, and the fiber of base cloth fabric is intact, high-performance transparent adhesive can be used to paste or heat seal in the worn area.
2、如果膜面破坏范围长度小于50mm,剪一椭圆形或圆形膜布,作为补强层焊接在破坏区域的上面。
2. If the length of the damage area of the membrane surface is less than 50mm, cut an oval or round membrane cloth and weld it on the damaged area as a reinforcement layer.
3、如果膜面破坏范围长度超过50mm但小于300mm,准备一长度和宽度比破坏范围大150mm的膜条,作为补强层焊接在破坏区域的膜面上。
3. If the length of the damage range of the membrane surface exceeds 50mm but is less than 300mm, prepare a membrane strip whose length and width are 150mm larger than the damage range, and weld it on the membrane surface of the damage area as a reinforcement layer.
山东膜结构
4、如果膜面破坏部分超过300mm长,需将整个破坏的单元拆下运回工厂修补或更换整个单元。
4. If the damaged part of the membrane surface is more than 300mm long, the entire damaged unit shall be removed and transported back to the factory for repair or replacement.
二、根据膜结构材料的不同,具体方法如下:
2、 According to different membrane structural materials, the specific methods are as follows:
1、PVC涂层覆盖的膜材料可采用热风机修补;将待补区域清理干净、铺放平整,补丁铺在待焊面上,用热风将膜材表面的PVC涂层融化,再将补丁与下层膜用小滚轮压机使其牢固地连在一起。而上述1至3的情况是现场修补,具体修补方法随所用膜材种类而定。
1. The membrane material covered by PVC coating can be repaired by hot air blower; Clean the area to be repaired, lay it flat, lay the patch on the surface to be welded, melt the PVC coating on the membrane surface with hot air, and then firmly connect the patch with the lower membrane with a small roller press. The above 1 to 3 cases are on-site repair, and the specific repair method depends on the type of membrane materials used.
2、对PTFE涂层覆盖的膜材,需在补丁与原破坏的膜材间加一层氟化乙丙烯薄膜;再用专用手提焊接设备压紧在补丁上,用高温使氟化乙丙烯薄膜融化从而将补丁焊接在膜面上。具体操作时要注意加热温度和加热时间的把握,既要使待焊膜材的表面涂层或FEP薄膜充分融化从而能牢固粘在一起,又要防止因过热而烧焦膜材。
2. For the membrane material covered by PTFE coating, a layer of FEP film shall be added between the patch and the original damaged membrane material; Then press the patch with special portable welding equipment, melt the FEP film with high temperature, and weld the patch on the film surface. During specific operation, pay attention to the control of heating temperature and heating time, not only to fully melt the surface coating or FEP film of the film material to be welded so as to firmly stick together, but also to prevent the film material from burning due to overheating.
景观膜结构膜面破损的处理方式以及其他内容的了解就讲解到这里了,您对此有什么疑问要解答吗?欢迎来我们网站http://www.sdcscp.com咨询了解!
This is the end of our understanding of how to deal with the damage of the membrane surface of the landscape membrane structure and other contents. Do you have any questions to answer? Welcome to our website http://www.sdcscp.com Ask about it!
图标分类中心

Product

联系我们
青岛亿金来钢膜结构安装修缮工程有限公司 青岛亿金来钢膜结构安装修缮工程有限公司

联系电话:15694496888

联系地址:山东省青岛市城阳区前海西社区居委会西100米